Polymer Property : Melt Flow = 14.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 14.0 g/10 min
14.0 g/10 min
ASTM D1238
S&E Specialty Polymers TufGuard M™ GPP1005M-EXLT PP, Flame Retardant
Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers
Melt Flow 14.0 - 64.0 g/10 min
14.0 - 64.0 g/10 min
Average value: 39.7 g/10 min Grade Count:8
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Elexar® EL 3954-70 Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Elexar® EL 3954-90 Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1320E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 14.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
14.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1358C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2374A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-3955B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 14.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
14.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBW2492 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Uses: Film; Sheet Forms: Pellets Processing Method: Injection Molding;..
Melt Flow 14.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4975F Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Melt Flow 14.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
14.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-1431B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Terraloy™ MB 18003A Thermoplastic Starch + HIPS
Notes: Terraloy™ MB-18003A is a Thermoplastic Starch/HIPS masterbatch that contains up to 30% of TPS renewable content. High Impact PS Melt Index for the masterbatch is 9.8. This compound is inte..
Melt Flow 14.0 g/10 min

@Load 2.16 kg,
Temperature 200 °C
14.0 g/10 min

@Load 4.76 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Uniprene® UN-1011A Thermoplastic Elastomer
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-8732 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-8732R Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstri..
Melt Flow 14.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
14.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade
Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali
Melt Flow 14.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Elexar® EL 3954-80 Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti..
Melt Flow 14.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
14.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade
Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali