Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12.08 g/10 min @Load 10.0 kg, Temperature 380 °C |
12.08 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-8167 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Melt Flow | 12.08 g/10 min @Load 5.00 kg, Temperature 345 °C |
12.08 g/10 min @Load 11.0 lb, Temperature 653 °F |
|
Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy.. |