Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11.3 g/10 min @Load 6.60 kg, Temperature 337 °C |
11.3 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2110 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 11.3 g/10 min @Load 6.60 kg, Temperature 337 °C |
11.3 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Melt Flow | 11.3 g/10 min @Temperature 230 °C |
11.3 g/10 min @Temperature 446 °F |
|
Cyclewood Solutions Xylomer™ XM2-CUA Sustainable Injection Molding Resin 100% biodegradable and compostable thermoplastic. The sustainable bio-based resin properties perform between polypropylene and polystyrene. Xylomer™ is modified lignin, an abundant, natural bypro.. |
|||
Melt Flow | 11.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
11.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termite.. |
|||
Melt Flow | 11.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
11.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Dry) Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termite.. |
|||
Melt Flow | 11.3 g/10 min @Load 6.60 kg, Temperature 337 °C |
11.3 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |