Physical Properties Metric English Comments
Melt Flow 0.50 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1401D (Q30P) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 0.60 - 0.90 g/10 min
0.60 - 0.90 g/10 min
±12%
Kazanorgsintez 175-225 Film Grade Composition of High Density Polyethylene
Production Method: Based on polyethylene grades 10803-20, 15803-20, 15813-020,17504-006. Application: Designed for packing manufacture for milk and milk products.Information Provided by Kazanorg..
Melt Flow 0.60 - 0.90 g/10 min
0.60 - 0.90 g/10 min
±12%
Kazanorgsintez 175-76 Film Grade Composition of High Density Polyethylene
Production Method: Based on polyethylene grades 10803-20, 15803-20, 15813-020,17504-006. Application: Designed for packing manufacture for milk and milk products.Information Provided by Kazanorg..
Melt Flow 0.70 - 0.90 g/10 min

@Load 2.61 kg,
Temperature 190 °C
0.70 - 0.90 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC EF320 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical
Melt Flow 0.60 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem LB 0117 LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Melt Flow 0.60 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem LB 0120 BP LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Melt Flow 0.60 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem LB 0120 BPS LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Melt Flow 0.60 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem LB 0120 BS LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Melt Flow 0.60 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem LBH 0117 LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Melt Flow 0.60 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem LBH 0120 BPS LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Melt Flow 0.60 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem LBH 0120 BP LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Melt Flow 0.60 - 0.90 g/10 min

@Load 5.00 kg,
Temperature 230 °C
0.60 - 0.90 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Kureha KF Polymer 1300 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Melt Flow 0.70 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Breplast Bretene HD Bottles Thin Flakes High Density Polyethylene
Recovered polyethylene compositeInformation provided by Breplast S.p.A.
Melt Flow 0.70 - 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 - 0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Breplast Bretene RD 90 High Density Polyethylene
Recovered polyethylene compositeInformation provided by Breplast S.p.A.