Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.40 - 0.80 g/10 min | 0.40 - 0.80 g/10 min | ±10% |
Kazanorgsintez PE80B-285 High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Melt Flow | 0.40 - 0.80 g/10 min | 0.40 - 0.80 g/10 min | ±10% |
Kazanorgsintez PE80B-285D High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Melt Flow | 0.40 - 0.80 g/10 min | 0.40 - 0.80 g/10 min | ±10% |
Kazanorgsintez PE80B-285SL High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Melt Flow | 0.30 - 0.80 g/10 min | 0.30 - 0.80 g/10 min | |
Zhejiang Juner PP201-G30 PP For Automotive Parts Applications: FansInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Breplast Bretene TS COR HF Film Light High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Breplast Bretene TS COR HF T10 Light High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Breplast Bretene TS COR HF Dark High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Breplast Bretene TS COR HF Film Dark High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |