Polymer Property : Melt Flow = 0.58 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.58 g/10 min
0.58 g/10 min
Kraton® D1102 + HDPE blend (15/85)
Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..
Melt Flow 0.58 g/10 min
0.58 g/10 min
ASTM D1238
Solvay Engineered Polymers DEXFLEX® E160 TPO  (discontinued **)
Description: DEXFLEX® E160 thermoplastic olefinic elastomer (TPO) is designed for extrusion applications that require thermal stability, excellent low-temperature properties, and good dimensional s..
Melt Flow 0.58 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.58 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras..