Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.33 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 15A Butene HDPE Film Resin Film Properties. Features: Low gel, good barrier properties, strength and toughness.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Flow | 0.33 g/10 min | 0.33 g/10 min | I<sub>2</sub>; ASTM D1238 |
Petromont 1000 High Density Polyethylene Resin Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to .. |
|||
Melt Flow | 0.33 g/10 min | 0.33 g/10 min | I<sub>2</sub>; ASTM D1238 |
Petromont 1002 High Density Polyethylene Resin Petromont HDPE 1002 is a blow moulding high-density polyethylene copolymer resin produced using the UNIPOL® Process. This multi-purpose resin can be used on intermittent and continuous extrusion bl.. |
|||
Melt Flow | 0.33 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem BT 003 HDPE Blow Molding Polyethylene
(discontinued **) Applications: Bottles for food products, lubricating and cooking oil; toys; bottler for surface-active agents; sheets. Information provided by Braskem |
|||
Melt Flow | 0.33 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos B53-35H-100 HDPE B53-35H-100 is a high density polyethylene copolymer developed for injection blow molding. Zinc Stearate is incorporated in the formulation as a release agent. It is recommended for use in applica.. |
|||
Melt Flow | 0.33 g/10 min | 0.33 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® LP510300 High Density Polyethylene ApplicationsPETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is r.. |
|||
Melt Flow | 0.33 g/10 min | 0.33 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® LP510300 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP510300 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. LP510300 is recommended .. |
|||
Melt Flow | 0.33 g/10 min | 0.33 g/10 min | ASTM D1238 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend Part.. |
|||
Melt Flow | 0.33 g/10 min | 0.33 g/10 min | ASTM D1238 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade) Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm.. |
|||
Melt Flow | 0.33 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Paxon™ AF50-003 Blow Molding Resin AProduct Description: AF50-003 is a blow molding high density polyethylene copolymer containing an antistatic additive. It offers very good balance of stress crack resistance, stiffness and impact s.. |