Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.070 g/10 min | 0.070 g/10 min | I<sub>2</sub>; ASTM D1238 |
Petromont 2001 High Density Polyethylene Resin Petromont HDPE 2001 is a high-density polyethylene copolymer resin produced using the UNIPOL ® Process. This resin has been designed specifically for film for various applications such as notion an.. |
|||
Melt Flow | 0.070 g/10 min | 0.070 g/10 min | ASTM D1238 |
LyondellBasell Alathon® L5008 High Density Polyethylene ApplicationsALATHON L 5008 is a high molecular weight high density polyethylene copolymer resin with broad and bimodal molecular weight distribution.Regulatory StatusWhen L 5008 is compounded with a.. |
|||
Melt Flow | 0.070 g/10 min | 0.070 g/10 min | ASTM D1238 |
LyondellBasell Alathon® L5008HP High Density Polyethylene, Pressure Pipe Extrusion Grade ALATHON L5008HP is a bimodal, high molecular weight, high density polyethylene resin with excellent processability designed to meet the high performance requirements of pressure pipe applications in.. |
|||
Melt Flow | 0.070 g/10 min | 0.070 g/10 min | |
JPJ Technologies 7300M HDPE Extrusion Information provided by JPJ Technologies |
|||
Melt Flow | 0.070 g/10 min @Load 2.16 kg |
0.070 g/10 min @Load 4.76 lb |
ASTM D1238 |
Equate EMDA-6147 HDPE Blow Molding Resin EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density.. |
|||
Melt Flow | 0.070 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.070 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® E927 Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin For Thin Film Applications Formolene® E927 is a high molecular weight grade of HDPE designed for high drawdown to produce thin films w.. |
|||
Melt Flow | 0.070 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.070 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® E927ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E927ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |