Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 21MB777 OPP Film Product Description: Bicor 21MB777 is a high gas barrier, biaxially oriented transparent PP film coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging m.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 25ICT OPP Film Product Description: A one-side sealable, very broad seal range coextruded BOPP. This film is designed for use in unsupported plain or surface printed high-speed horizontal applications. The enhance.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 25MB400 OPP Film Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 25MB666 OPP Film Product Description: A Biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 25MB668 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low seal temperature (VLTS) coating. VLTS coating provides excellent perf.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 25MB866 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side PVOH. It provides excellent gas and aroma protection and is designed to be use.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 25MBT666 OPP Film Product Description: Biaxially oriented polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping offering unique aspect and cost reduction advant.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 26MB600 OPP Film Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 36MO747 OPP Film Product Description: A white opaque biaxially oriented polypropylene film acrylic coated on one side, one side PVdC. Provides outstanding performances on all packaging machines.Availability: Africa .. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 38MO447 OPP Film Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film, heat sealable on the inside. The treated layer must be printed and varnished to provide the necess.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 38MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MW648 OPP Film Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides an excel.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 30MD447 OPP Film Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 30MW747 OPP Film Product Description: White opaque biaxially oriented polypropylene film coated on one side acrylic, one side PVdC. Provides excellent performances on all packaging machines. 30MW747 is a super white.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 35HM247 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial.. |
|||
Water Vapor Transmission | 1.10 g/m²/day @Temperature 23.0 °C |
0.0710 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MW647 OPP Film Product Description: A super white opaque, biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performance on all types of packaging machines.Availability: Africa & .. |