Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 341 SUS | 341 SUS | |
ChevronTexaco Alcaid® 60 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |
|||
Saybolt Viscosity at 100°F | 341 SUS | 341 SUS | |
ChevronTexaco ISO 68 Utility Oil LVI FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc.. |
|||
Saybolt Viscosity at 100°F | 341 SUS | 341 SUS | ASTM D445 |