Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 200 SUS | 200 SUS | Base Oil Viscosity |
Dow Corning MOLYKOTE® BG-20 SYNTHETIC BEARING GREASE Polyol Ester grease especially for high speed bearingsFeatures: Lubricating bearings operating under a wide range of conditions, including high speeds, extreme temperatures and high loads. Handles .. |
|||
Saybolt Viscosity at 100°F | 200 SUS | 200 SUS | |
ChevronTexaco Bright-Cut® NM Metal Working Fluid FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components .. |
|||
Saybolt Viscosity at 100°F | 200 SUS | 200 SUS | |
ChevronTexaco Elite-Cut® NH Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Saybolt Viscosity at 100°F | 200 SUS | 200 SUS | |
ChevronTexaco Elite-Cut® NM Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Saybolt Viscosity at 100°F | 200 SUS | 200 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® 783-0 Series Synthetic Food Grade Greases, NLGI Grade 0 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Saybolt Viscosity at 100°F | 200 SUS | 200 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® 783-00 Series Synthetic Food Grade Greases, NLGI Grade 00 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Saybolt Viscosity at 100°F | 200 SUS | 200 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® 783-1 Series Synthetic Food Grade Greases, NLGI Grade 1 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Saybolt Viscosity at 100°F | 200 SUS | 200 SUS | |
ConocoPhillips Hydroclear® ATF Type F Automatic Transmission Fluid Description: Conoco Hydroclear ATF Type F Automatic Transmission Fluid is a high-static-friction fluid developed for Ford automatic transmissions manufactured during the 1960s and 1970s. (Newer Ford.. |