Polymer Property : Apparent Bulk Density = 0.750 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPAS® 6605 MP Melamine
Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be..
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Apparent Bulk Density 0.670 - 0.750 g/cc
0.0242 - 0.0271 lb/in³
IS 867-1963
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow ..
Apparent Bulk Density 0.700 - 0.750 g/cc
0.0253 - 0.0271 lb/in³
IS 867-1963
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R..
Apparent Bulk Density 0.700 - 0.750 g/cc
0.0253 - 0.0271 lb/in³
IS 867-1963
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R..
Apparent Bulk Density 0.550 - 0.750 g/cc
0.0199 - 0.0271 lb/in³
ISO 60
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..