Physical Properties Metric English Comments
Apparent Bulk Density 0.290 - 0.300 g/cc
0.0105 - 0.0108 lb/in³
Average value: 0.298 g/cc Grade Count:8
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report..
Apparent Bulk Density 0.200 - 0.300 g/cc
0.00723 - 0.0108 lb/in³
IS 867-1963
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa..