Physical Properties Metric English Comments
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
ASTM D1895
Solvay Specialty Polymers Algoflon® L101-1 Polytetrafluoroethylene (PTFE)
Algoflon® L101-1 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It exhibits excellent chemical and heat resistance, low surface energy and low coefficien..
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F..
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
Cosmic Plastics 6230 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
Cosmic Plastics K66 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
Tap density
Carborundum CarboTherm™ CTF10 Boron Nitride Powder
Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect..
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
Tap density
Carborundum CarboTherm™ CTF5 Boron Nitride Powder
Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect..
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
ASTM D4895
Solvay Specialty Polymers Algoflon® L101-1 Polytetrafluoroethylene (PTFE)  (Unverified Data**)
Algoflon® L101-1 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It exhibits excellent chemical and heat resistance, low surface energy and low coefficient ..
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
Cosmic Plastics D62 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound