Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.380 g/cc | 0.0137 lb/in³ | Geon® STP 1169; Internal Method |
PolyOne Geon™ Specialty Suspension CG E 24 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® CG E24 is a homopolymer specialty suspension resin intended for use in controlling gloss and transparency of injection molded, extruded or plastisol parts. This resin provides low surface glo.. |
|||
Apparent Bulk Density | 0.380 g/cc | 0.0137 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® F 5 Polytetrafluoroethylene (PTFE) Algoflon® F 5 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for filled grades and in particular is recommended for compounds with glass fiber .. |
|||
Apparent Bulk Density | 0.380 - 0.700 g/cc | 0.0137 - 0.0253 lb/in³ | Average value: 0.535 g/cc Grade Count:4 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |