Polymer Property : Viscosity = 9300 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 9300 - 9300 cP

@Temperature 190 - 190 °C
9300 - 9300 cP

@Temperature 374 - 374 °F
Average value: 9300 cP Grade Count:1
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..