Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 9300 cP @Shear Rate 11200 1/s, Temperature 200 °C |
9300 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Viscosity | 9300 cP @Shear Rate 11200 1/s, Temperature 200 °C |
9300 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Viscosity | 9300 - 9300 cP @Temperature 190 - 190 °C |
9300 - 9300 cP @Temperature 374 - 374 °F |
Average value: 9300 cP Grade Count:1 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Viscosity | 9300 cP @Temperature 190 °C |
9300 cP @Temperature 374 °F |
melt viscosity; ASTM D-3236 |
ExxonMobil Escorene® LD-770 Very High Flow EVA Resin for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A relatively low viscosity ethylene vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance, at the same viscosity of.. |
|||
Viscosity | 9300 cP @Temperature 190 °C |
9300 cP @Temperature 374 °F |
ASTM D3236 |
ExxonMobil Escorene® UL 8705 Adhesive Application Resin Escorene Ultra UL 8705 is a relatively low viscosity, 27.6% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has .. |
|||
Viscosity | 9300 cP @Temperature 190 °C |
9300 cP @Temperature 374 °F |
ASTM D3236 |
ExxonMobil Escorene® UL 8705E Adhesive Application Resin Escorene Ultra UL 8705 is a relatively low viscosity, 29% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has go.. |
|||
Viscosity | 9300 - 10700 cP @Temperature 35.0 °C |
9300 - 10700 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G173 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 9300 cP | 9300 cP | Mixed - low; Resin - 9,300 cP; Hardener - 2,700 cP |
Loctite® Durabond® E-00CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |