Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 92000 cP | 92000 cP | Melt Viscosity, 250°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® SHF4960 PBT Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Viscosity | 92000 cP @Temperature 204 °C |
92000 cP @Temperature 399 °F |
Melt; ASTM D1084-88 |
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv.. |
|||
Viscosity | 92000 cP | 92000 cP | A Component; ASTM D1824 |
Aptek 2209-A/B Clear, non-yellowing urethane adhesive APTEK 2209-A/B is a water clear, thixotropic, two component, electrically insulating, urethane adhesive designed for bonding various substrates. APTEK 2209-A/B is effective for bonding plastics and.. |