Physical Properties Metric English Comments
Viscosity 850 cP
850 cP
Reltek BONDiT™ HM-502 Coating, Sealant, Adhesive System
A protective coat for most metal, glass, and ceramic materials for use against corrosion and other chemical attacks. Useful against fungi growth. Bondit HM-502 is a thermoplastic emulsion system.Inf..
Viscosity 850 cP
850 cP
Reltek BONDiT™ HM-505 Coating, Sealant, Adhesive System
Information provided by Reltek LLC
Viscosity 850 cP

@Temperature 23.0 °C
850 cP

@Temperature 73.4 °F
25% in NMP
Solvay Specialty Polymers Torlon® AI-10 LM Polyamide-imide (PAI)  (Unverified Data**)
Torlon AI-10 LM is a polyamide-imide (PAI) powder developed for the performance coatings industry. It is similar to Torlon AI-10 in that it is produced using the same monomers and polymerization sys..
Viscosity 850 cP

@Temperature 25.0 °C
850 cP

@Temperature 77.0 °F
Struktol STRUKSILON 8015 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8015 is a specifically designed silicone stabilizer for appliance application and other applications where good flowability is required, like pipe insulation and hot water boiler producti..
Viscosity 850 cP

@Temperature 160 °C
850 cP

@Temperature 320 °F
Melt; ETM 22-31
ExxonMobil ESCOREZ™ 5600 Petroleum Hydrocarbon Resin
Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and metallocene polyolefines. Avail..
Viscosity 850 cP

@Temperature 25.0 °C
850 cP

@Temperature 77.0 °F
Cytec CC-1191 (Conap) Acrylic Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Viscosity 850 cP

@Temperature 25.0 °C
850 cP

@Temperature 77.0 °F
Cytec CE-1171 (Conap) Acrylic Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Viscosity 850 cP
850 cP
dynamic
Dow Corning 3-6512 A&B ELASTOMER
Two-part, transparent, 1:1, moderate heat cure, long pot life, cures to soft elastomer.Information provided by Dow Corning
Viscosity 850 cP
850 cP
25% Toluene Solution at 25°C; BAM 922
Kraton® D4150 K (O/E SBS) Linear Triblock Copolymer
Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton..