Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 800 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 400 - 800 cP

@Temperature 25.0 °C
400 - 800 cP

@Temperature 77.0 °F
cPs
Oceanchem Group Resorcinol bis (Diphenyl Phosphate) (RDP)
Molecular Formula: C30H24O8P2Cas No.: 57583-54-7RDP is a halogen-free phosphorus-based flame retardant.Use:RDP flame retardant provides a halogen-free solution for flame retarding PC/ABS, PPO/HIPS a..
Viscosity 400 - 800 cP
400 - 800 cP
ND Industries 560 Shaft & Bearing Retainer Retaining Compound
High Temperature retainer for bushings and sleeves. Retains rotors to shaftsMeets military spec Mil-R-46082B Type II
Viscosity 300 - 800 cP
300 - 800 cP
Huntsman AroCy M-20 Monomeric Bisphenol F Dicyanate
Comments/Applications: Low melt viscosity coprepolymer of M-30/B-30 type materials. RTM, unidirectional prepreg manufacture for radomes, high gain antennas and high density circuitry.Data provided ..
Viscosity 100 - 800 cP
100 - 800 cP
ASTM D803
SK Chemicals SKYTHANE® UB220 Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Viscosity 500 - 800 cP
500 - 800 cP
Solvay IGEPAL® CA 210 Surfactant
Description: Octyl phenol ethoxylate (1.5EO). Effective emulsifier for nonpolar solvents in solvent emulsion cleaners, pesticides, dry cleaning detergents and floor polishes. Nonionic dispersant and..
Viscosity 120 - 800 cP
120 - 800 cP
20% solids in MEK
Taiwan Sheen Soon Sheenthane® AS-330 TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo..
Viscosity 200 - 800 cP
200 - 800 cP
#2 sp @ 30 rpm; RP-0596
Solvay RHODOLINE® 681-F Surfactant
Description: Mineral oil defoamers for high PVC systems.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: For best results, RHODOLINE© 681-F should be used as received. As..
Viscosity 600 - 800 cP
600 - 800 cP
Epoxyset Epoxibond EB-106 Unfilled Epoxy Adhesive
A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc.
Viscosity 550 - 800 cP

@Temperature 35.0 °C
550 - 800 cP

@Temperature 95.0 °F
Dynamic viscosity
C.O.I.M. PLAXTER® P 72 Polymeric Plasticizer
Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc.
Viscosity 400 - 800 cP
400 - 800 cP
Mixed Viscosity
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Viscosity 600 - 800 cP
600 - 800 cP
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone
Viscosity 600 - 800 cP
600 - 800 cP
Aremco HiE-Coat™ 840-CM High Emissivity Coating, Inorganic-Ceramic Filled
Ceramic-based, black-pigmented coating for dense refractories to 2500°F (1371°C) and stainless steel to 900°F (482°C)
Viscosity 600 - 800 cP
600 - 800 cP
Aremco Pyro-Paint™ 634-AS High Temperature Refractory Coating
This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting ..
Viscosity 100 - 800 cP
100 - 800 cP
3M Scotch-Weld™ Hi-Strength Laminating 92 Spray Adhesive
A high performance, high temperature resistant, tack industrial grade spray adhesive designed for use in a wide variety of applications.Features:It can be used for high pressure laminate, veneers, f..
Viscosity 400 - 800 cP
400 - 800 cP
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a..
Viscosity 100 - 800 cP
100 - 800 cP
Beijing Ranger Chem SM-828A90 Solvent Based Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 300 - 800 cP
300 - 800 cP
LV# @ 60 rpm; RP-0596
Solvay RHODOLINE® 670 Surfactant
Description: Highly effective mineral oil defoamer for latex processing..Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE 670 is an APE-free and silicone–free def..