Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 76000 cP @Temperature 25.0 °C |
76000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 868-3N1 Room Temperature Cure Adhesive TRA-BOND 868-3N1 room temperature cure adhesive provides strong bonds to difficult-to-bond metals, such as gold, silver, copper, brass, and solder.Information provided by Tra-Con Inc. |
|||
Viscosity | 76000 cP | 76000 cP | dynamic |
Dow Corning SE 4400 KIT Two-part, grey, heat cure, flowable, thermally conductive, UL V-0.Information provided by Dow Corning |
|||
Viscosity | 76000 cP | 76000 cP | B Component; ASTM D1824 |
Aptek 2209-A/B Clear, non-yellowing urethane adhesive APTEK 2209-A/B is a water clear, thixotropic, two component, electrically insulating, urethane adhesive designed for bonding various substrates. APTEK 2209-A/B is effective for bonding plastics and.. |