Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 750 cP @Temperature 82.2 °C |
750 cP @Temperature 180 °F |
|
Northstar Polymers MSA-042 Polyester Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 750 cP | 750 cP | |
Resinlab® CYNERGY CA6008 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 750 cP | 750 cP | |
Resinlab® RC8041 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Viscosity | 750 cP | 750 cP | |
Resinlab® CYNERGY CA6808 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 750 cP | 750 cP | Fed Std Method 4287 |
Humiseal 1B31LSE Acrylic Conformal Coating Humiseal 1B31LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C Approval PendingPasses thermal sho.. |
|||
Viscosity | 750 cP @Temperature 25.0 °C |
750 cP @Temperature 77.0 °F |
Mixed; STM 1 |
Lord Adhesives Thermoset™ UR-322 Two Component Urethane Potting Compound Lord UR-322 is a two component, room temperature curing urethane potting compound. The cured elastomer is soft, flexible and has a very low modulus at temperatures down to -80°C. Cured UR-322 als.. |
|||
Viscosity | 750 - 1450 cP | 750 - 1450 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1102 E (SBS) Liner Block Copolymer Description: Kraton D1102 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 28.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Viscosity | 750 - 1250 cP | 750 - 1250 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1111 K (SIS) Linear Triblock Copolymer Description: Kraton D1111 K is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: .. |
|||
Viscosity | 750 cP @Temperature 25.0 °C |
750 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6126 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 750 cP @Temperature 25.0 °C |
750 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6136 Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 750 cP @Temperature 25.0 °C |
750 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6156 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 750 cP @Temperature 25.0 °C |
750 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6166 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 750 cP @Temperature 25.0 °C |
750 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6186 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 750 cP @Temperature 25.0 °C |
750 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6196 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 750 cP | 750 cP | |
Von Roll Isola IMI Varnish 712 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa.. |
|||
Viscosity | 750 cP | 750 cP | dynamic |
Dow Corning Q3-6575 DIELECTRIC GEL A/B KIT Two-part, clear, RT or heat cure and low temperature (-80°C/-112°F)stability.Information provided by Dow Corning |
|||
Viscosity | 750 cP @Temperature 160 °C |
750 cP @Temperature 320 °F |
Melt; ETM 22-31 |
ExxonMobil ESCOREZ™ 1310 LC Petroleum Hydrocarbon Resin This product is a light colored, premium aliphatic hydrocarbon resin with narrow molecular weight distribution. It is designed to tackify a variety of adhesive polymers including EVA, metallocene .. |
|||
Viscosity | 750 cP @Temperature 160 °C |
750 cP @Temperature 320 °F |
Melt; ETM 22-31 |
ExxonMobil Escorez™ 2203LC (AM & EU) Tackifying Resin Product Description: Escorez™ 2203LC is a premium aromatic modified aliphatic hydrocarbon resin with a narrow molecular weight distribution. It is characterized by low color and low volatility. It.. |
|||
Viscosity | 750 cP | 750 cP | Hardener |
ACC EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast.. |
|||
Viscosity | 750 cP | 750 cP | Resin |
ACC EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast.. |
|||
Viscosity | 750 - 950 cP | 750 - 950 cP | |
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Viscosity | 750 - 2000 cP | 750 - 2000 cP | |
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating This advanced silicon carbide, water-based coating reduces significantly the oxidation of graphite and carbon components and structures at temperatures to 2550 °F (1400 °C). Provides a hard surfac.. |
|||
Viscosity | 750 cP | 750 cP | Side B |
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti.. |
|||
Viscosity | 750 - 1250 cP | 750 - 1250 cP | |
Aremco Ceramacoat™ 845-GLT High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, light-green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps,.. |
|||
Viscosity | 750 cP @Temperature 25.0 °C |
750 cP @Temperature 77.0 °F |
Uncured |
Permabond A025 Anaerobic Retainer Permabond® A025 is an anaerobic adhesive formulated to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It has been designed for ap.. |
|||
Viscosity | 750 cP | 750 cP | B Side |
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst.. |
|||
Viscosity | 750 cP | 750 cP | ASTM D2293 |
Fibre Glast EZ Poxy EZ10 / EZ83 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |