Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 200000 - 700000 cP @Temperature 400 - 420 °C |
200000 - 700000 cP @Temperature 752 - 788 °F |
Average value: 445000 cP Grade Count:13 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Viscosity | 350000 - 700000 cP | 350000 - 700000 cP | |
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4.. |