Polymer Property : Viscosity = 620000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 620000 cP

@Temperature 160 °C
620000 cP

@Temperature 320 °F
Melt viscosity @ 2.16 kg; ISO 1133
Lubrizol Advanced Materials Pearlbond® 180 Thermoplastic Polyurethane
Pearlbondâ„¢ 180 is a linear, polyester-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. It i..