Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 6200 cP @Shear Rate 11200 1/s, Temperature 200 °C |
6200 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod.. |
|||
Viscosity | 6200 cP @Shear Rate 11200 1/s, Temperature 200 °C |
6200 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Viscosity | 6200 cP @Shear Rate 11200 1/s, Temperature 200 °C |
6200 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp.. |
|||
Viscosity | 6200 cP @Temperature -20.0 °C |
6200 cP @Temperature -4.00 °F |
Cold Cranking |
ConocoPhillips Conoco® El Mar® Ashless Supreme Oil, SAE Viscosity Grade 15W-40 Conoco® El Mar Ashless Supreme is a premium quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and turbocharged 2-stroke cycle natural gas engines. Engine.. |
|||
Viscosity | 6200 cP @Shear Rate 10994 1/s, Temperature 210 °C |
6200 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7140-1000 TPE Product Description: StarFlex P 7140-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Viscosity | 6200 cP | 6200 cP | Mixed - low; Resin - 6,200 cP; Hardener - 13,000 cP |
Loctite® Durabond® E-60NC Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |