Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 560000 cP | 560000 cP | |
Dow Corning SILASTIC® 9280/70E KIT PARTS A&B 70 Durometer, 2 parts, 1 to 1 mix, translucent, injection molding grade Liquide Silicone Rubber.Information provided by Dow Corning |
|||
Viscosity | 560000 cP @Temperature 260 °C |
560000 cP @Temperature 500 °F |
Melt Viscosity; DSM method |
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |