Polymer Property : Viscosity = 55000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 3000 - 55000 cP
3000 - 55000 cP
Average value: 18000 cP Grade Count:5
Overview of materials for Silicone Foam
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW..
Viscosity 45000 - 55000 cP
45000 - 55000 cP
dynamic
Dow Corning Q3-3559 SEMIFLOWABLE TEXTILE ELASTOMER
A semi-flowable 1 part solventless silicone elastomer.Information provided by Dow Corning
Viscosity 35000 - 55000 cP
35000 - 55000 cP
Epoxyset Epoxiohm EO-98HT Electrically Conductive Epoxy Adhesive
EO-98HT is a one component, electrically and thermally conductive, snap cure, die attach epoxy. It was designed for IC plastic packaging of semiconductors, hybrid micro-electronics, and photonic dev..
Viscosity 35000 - 55000 cP
35000 - 55000 cP
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Viscosity 15000 - 55000 cP
15000 - 55000 cP
Lord Adhesives 201 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f..