Polymer Property : Viscosity = 550 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 550 - 350000 cP
550 - 350000 cP
Average value: 27500 cP Grade Count:27
Overview of materials for Epoxy Adhesive, Flexible
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro..
Viscosity 550 - 850 cP
550 - 850 cP
Huntsman Euredur 43 S Cycloaliphatic Amine
Approx. H+ equivalent weight 115. Mix Ratio with GY 6010 is 60.Comments/Applications: Euredur 43 S is the accelerated version of Euredur 43.Data provided by Ciba Specialty Chemicals.Ciba Specialty..
Viscosity 550 - 850 cP
550 - 850 cP
Huntsman MY 0510 Multifunctional Resin
Weight per Epoxide (EEW, g/eq) 95 to 107. Color: BrownComments/Applications: High purity MY 0500. Improved stability. Boosts performance of bisphenol A resins. Used for rapid cure adhesives, lam..
Viscosity 550 - 850 cP

@Temperature 125 °C
550 - 850 cP

@Temperature 257 °F
542-111
Westlake Epolene® N-35 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-35 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Viscosity 550 cP

@Temperature 30.0 °C
550 cP

@Temperature 86.0 °F
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure
DescriptionDSM Somos® 12120 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12120 have a cherry-red appearance which tur..
Viscosity 550 - 750 cP
550 - 750 cP
Dow CYRACURE™ UVR-6128 Cycloaliphatic Epoxide
CYRACURE™ UVR-6107 cycloaliphatic epoxide is a standard flexibilizing cycloaliphatic epoxide resin. Typical applications include: Metal decoration coatings Overprint varnishes Flexible packaging ..
Viscosity 550 cP
550 cP
dynamic
Dow Corning 3-4154 DIELECTRIC GEL KIT
Two-part, clear, RT or heat cure.Information provided by Dow Corning
Viscosity 550 - 700 cP

@Temperature 35.0 °C
550 - 700 cP

@Temperature 95.0 °F
Dynamic viscosity
C.O.I.M. PLAXTER® P 70 Polymeric Plasticizer
Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc.
Viscosity 550 - 800 cP

@Temperature 35.0 °C
550 - 800 cP

@Temperature 95.0 °F
Dynamic viscosity
C.O.I.M. PLAXTER® P 72 Polymeric Plasticizer
Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc.
Viscosity 550 cP
550 cP
B Side
ACC EP RAP-1567 EPI Engineered Polymers Aliphatic Polyurea
RAP-1567 HX is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generat..
Viscosity 550 cP
550 cP
B Side
ACC EP RAP-1567 HX EPI Engineered Polymers Aliphatic Polyurea
RAP-1567 is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation..
Viscosity 550 cP
550 cP
B Side
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea
RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This ne..
Viscosity 550 cP
550 cP
B Side
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea
RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This..
Viscosity 550 - 750 cP
550 - 750 cP
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester
Viscosity 550 cP
550 cP
Abatron AboCast 50-3/AboCure 8110-1 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..
Viscosity 550 cP
550 cP
Dymax 3069 Solvent-Free Plastic Adhesive
Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide ..