Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 534000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
534000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; Internal Method |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-re.. |
|||
Viscosity | 534000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
534000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes.. |