Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5.00e+6 - 2.50e+7 cP | 5.00e+6 - 2.50e+7 cP | |
Lord Adhesives 304 General Purpose, High Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 5.00e+6 cP @Shear Rate 0.100 1/s, Temperature 240 °C |
5.00e+6 cP @Shear Rate 0.100 1/s, Temperature 464 °F |
|
DSM Akulon® XP36-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 5.00e+6 cP @Shear Rate 0.100 1/s, Temperature 240 °C |
5.00e+6 cP @Shear Rate 0.100 1/s, Temperature 464 °F |
|
DSM Akulon® XP36-E1 PA6 Film Extrusion, Medium Viscosity, Nucleated, Lubricated |