Physical Properties Metric English Comments
Viscosity 450 - 550 cP
450 - 550 cP
ND Industries StudGrade® 140 Permanent Threadlocker
General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m..
Viscosity 450 - 550 cP
450 - 550 cP
Liquid State
Palm Labs Adhesives TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED (500 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 150 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
Viscosity 450 - 550 cP
450 - 550 cP
Liquid State
Palm Labs Adhesives TURBO FUSE SERIES 130 CLEAR FLEXIBLE (100 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 150 CLEAR FLEXIBLE advanced formula is designed to polymerize instantly by absorbing surface moisture. The produ..
Viscosity 450 - 550 cP
450 - 550 cP
Liquid State
Palm Labs Adhesives Turbo Fuse Series 150 (500 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 150 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
Viscosity 450 cP

@Temperature 30.0 °C
450 cP

@Temperature 86.0 °F
DSM Somos® 9120 Epoxy Photopolymer  (Unverified Data**)
DescriptionDSM Somos® 9120 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p..
Viscosity 450 cP
450 cP
(mixed)
Loctite® Shadowcure™ 397 Acrylic/urethane Heat Cure Coating
Conformal CoatingsConformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Locti..
Viscosity 450 cP

@Temperature 30.0 °C
450 cP

@Temperature 86.0 °F
DSM Somos® 9120
The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp..
Viscosity 450 cP

@Temperature 25.0 °C
450 cP

@Temperature 77.0 °F
Esstech X-747-0000 Ethoxylated Bis Phenol A Dimethacrylate, C35H48O10
This form of EBPADMA has 6 units of ethoxylation. Increasing the ethoxylated chain length increases the mobility of the molecule and therefore it reactivity and degree of conversion. CAS # 41637-38-..
Viscosity 450 cP

@Temperature 25.0 °C
450 cP

@Temperature 77.0 °F
ACC EP AOSR EPI Engineered Polymers Acrylic Oligomer
EP AOSR, is an aliphatic triacrylate oligomer and is "Powered by Reactamine ®Technology”. EP AOSR is light in color and has fast cure response to UV and EB. EP AOSR exhibits good flexibility, toug..
Viscosity 450 cP
450 cP
A Side
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea
EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr..
Viscosity 450 cP
450 cP
A Side
ACC EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea
EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with supe..
Viscosity 450 cP
450 cP
A Side
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria..
Viscosity 450 cP
450 cP
A Side
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa..
Viscosity 450 - 650 cP
450 - 650 cP
blended
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v..
Viscosity 450 cP
450 cP
A Side
ACC EP RP EPI Engineered Polymers Aromatic Polyurea
EP RP, Aromatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RP displays extremely fast cure time..
Viscosity >= 450 cP
>= 450 cP
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Viscosity 450 cP
450 cP
Mixed (cp #40, 10 rpm)
Tra-Con Tra-Bond 516H01 Low Viscosity Room Temperature Cure Adhesive
TRA-BOND 516H01 is a room temperature curing, low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors, including Pre-Mixed and Frozen applications. It has also been use..