Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 45 cP | 45 cP | |
Resin Technology Group 345 General Purpose Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 345 General Purpose Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Viscosity | 45 cP | 45 cP | |
Resinlab® CYNERGY CA6004 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 45 cP | 45 cP | |
Resinlab® CYNERGY CA6804 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 45 cP @Temperature 20.0 °C |
45 cP @Temperature 68.0 °F |
2%, Hoppler |
Mikro-Technik 75a Carboxymethylcellulose (CMC) Technical GradeComments: All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E). Reduced active contents down to 50 % are available. Special conc.. |
|||
Viscosity | 45 cP | 45 cP | 5% max in styrene solution at 25°C; ASTM D455 |
Styron SE PB-3501 Schkopau Low-cis Polybutadiene Rubber (PBR) Composition: SE PB-3501 - Schkopau is a low-cis polybutadiene synthetic rubber. It is produced by anionic solution polymerization adjusted for a very high level of branching. SE PB-3501 - Schkopau i.. |
|||
Viscosity | 45 cP @Temperature 200 °C |
45 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3231 Polyester, Flake Molecular weight higher than UE3230, Improved solubilityUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as ad.. |
|||
Viscosity | 45 - 65 cP @Temperature 25.0 °C |
45 - 65 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 43 Heat Cure Catalyst Emerson & Cuming 43 Eccobond® Heat Cure CatalystRoom temperature gelling version of 28. Excellent for low stress potting and bonding. Will post cure in actual use. Combines the benefits of both 9 a.. |
|||
Viscosity | 45 cP | 45 cP | |
Loctite® 460 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 45 cP | 45 cP | |
Loctite® Super Bonder® 495 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 45 - 75 cP | 45 - 75 cP | |
BASF Lupranate® 273 Isocyanate Description: Lupranate® 273 Isocyanate is a solvent-free polymeric MDI with a functionality of approximately 2.3. Lupranate® 273 Isocyanate is a polymeric MDI which contains a relatively high leve.. |
|||
Viscosity | 45 cP | 45 cP | |
3M P597 Clear Teak & Glass Primer 3M™ Adhesion Promoter AP596 and 3M™ Primers P590, P591, P592, P595 and P597 are low viscosity adhesion promoters recommended for use with the 3M™ 500-Series Polyurethane Adhesives/Sealants and 3M.. |