Physical Properties Metric English Comments
Viscosity 380000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
380000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Viscosity 380000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
380000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and ..
Viscosity 380000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
380000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
Viscosity 380000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
380000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Viscosity 380000 cP

@Temperature 160 °C
380000 cP

@Temperature 320 °F
Melt viscosity @ 2.16 kg; ISO 1133
Lubrizol Advanced Materials PEARLBOND® 121 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 121 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit..
Viscosity 380000 cP

@Temperature 130 °C
380000 cP

@Temperature 266 °F
Melt; ISO 1133
Lubrizol Advanced Materials PEARLBOND® 523 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 523 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level...
Viscosity 380000 cP

@Temperature 160 °C
380000 cP

@Temperature 320 °F
Melt viscosity @ 2.16 kg; ISO 1133
Lubrizol Advanced Materials PEARLBOND® 101 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 101 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve..
Viscosity 380000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
380000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide..
Viscosity 380000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
380000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa..
Viscosity 380000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
380000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
Viscosity 380000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
380000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
Viscosity 380000 - 430000 cP
380000 - 430000 cP
Part A
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy
Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi..
Viscosity 380000 cP

@Shear Rate 1000 1/s,
Temperature 260 °C
380000 cP

@Shear Rate 1000 1/s,
Temperature 500 °F
melt viscosity; b.o. ISO 11443-A
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..
Viscosity 380000 cP
380000 cP
Victrex® PEEK 380P Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, medium flow, FDA food contact compli..
Copyright © lookpolymers.com All Rights Reserved