Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 380000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
380000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Viscosity | 380000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
380000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Viscosity | 380000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
380000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Viscosity | 380000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
380000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Viscosity | 380000 cP @Temperature 160 °C |
380000 cP @Temperature 320 °F |
Melt viscosity @ 2.16 kg; ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 121 Linear Thermoplastic Polyurethane Pearlbond™ 121 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Viscosity | 380000 cP @Temperature 130 °C |
380000 cP @Temperature 266 °F |
Melt; ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 523 Linear Thermoplastic Polyurethane Pearlbond™ 523 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Viscosity | 380000 cP @Temperature 160 °C |
380000 cP @Temperature 320 °F |
Melt viscosity @ 2.16 kg; ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 101 Linear Thermoplastic Polyurethane Pearlbond™ 101 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve.. |
|||
Viscosity | 380000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
380000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Viscosity | 380000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
380000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK) KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa.. |
|||
Viscosity | 380000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
380000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Viscosity | 380000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
380000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Viscosity | 380000 - 430000 cP | 380000 - 430000 cP | Part A |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
Viscosity | 380000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
380000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
Viscosity | 380000 cP | 380000 cP | |
Victrex® PEEK 380P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, medium flow, FDA food contact compli.. |