Polymer Property : Viscosity = 37000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 37000 cP
37000 cP
NextGen Adhesives G907-27 Structural Adhesive
Description: NGAC G907-27 is a medium viscosity polyamide adhesive system utilized extensively in industrial and structural applications.Advantages and Applications: The NGAC G907-27 provides excell..
Viscosity 37000 cP

@Temperature 25.0 °C
37000 cP

@Temperature 77.0 °F
Mixed
Trelleborg Emerson & Cuming Eccobond® 45 Two-Component General Purpose Epoxy Adhesive
Emerson & Cuming 45 Eccobond® Two-Component General Purpose Epoxy AdhesiveFilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of ..
Viscosity 37000 cP

@Temperature 25.0 °C
37000 cP

@Temperature 77.0 °F
After mixing
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive
TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc..
Viscosity 37000 cP
37000 cP
catalyzed with QM CAT 140
ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material
QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho..