Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 325000 cP @Temperature 400 °C |
325000 cP @Temperature 752 °F |
Melt; ISO 11443 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Viscosity | 325000 cP | 325000 cP | Part A, RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili.. |