Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 10 - 30 cP @Temperature 25.0 °C |
10 - 30 cP @Temperature 77.0 °F |
Uncured |
Permabond HL126 Anaerobic Threadlocker PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi.. |
|||
Viscosity | 10 - 30 cP | 10 - 30 cP | 0.5-10.0% solids |
Panipol Oy T Inherently Conductive Polymer Doped polyaniline in tolueneSolution Processing, Coating formulations, Ink formulationsInformation provided by Panipol Oy Ltd |
|||
Viscosity | 1.0 - 30 cP | 1.0 - 30 cP | ASTM D445 |
IRPC Polimaxx Polene PE100N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Viscosity | 10 - 30 cP | 10 - 30 cP | As Supplied |
Heraeus Cleviosâ„¢ PH Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH is an antistatic material based on PEDOT:PS.. |
|||
Viscosity | 15 - 30 cP | 15 - 30 cP | |
Shandong Dongyue Polymer DF-302 PTFE Aqueous Dispersion 60% Usage: The resin is used for impregnating porous material, such as asbestos, fiberglass, anti-corrosive, abrasion resistant, filature and lubricating materials.Packing: The PTFE is packed in PVC cir.. |
|||
Viscosity | 15 - 30 cP | 15 - 30 cP | |
Shandong Dongyue Polymer DF-301 PTFE Aqueous Dispersion 60% Usage: The resin is used for impregnating porous material, such as asbestos, fiberglass, anti-corrosive, abrasion resistant, filature and lubricating materials.Packing: The PTFE is packed in PVC cir.. |
|||
Viscosity | 20 - 30 cP @Temperature 25.0 °C |
20 - 30 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 23 LV General Purpose Catalyst Emerson & Cuming 23 LV Eccobond® General Purpose CatalystExcellent low temperature performance properties, excellent thermal shock/cycle and impact resistance. Good hardener for cryogenic applicati.. |
|||
Viscosity | 25 - 30 cP @Temperature 20.0 °C |
25 - 30 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 70-27 Polyvinyl Alcohol Intermediately Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 25 - 30 cP @Temperature 20.0 °C |
25 - 30 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 70-30 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 10 - 30 cP | 10 - 30 cP | dynamic |
Dow Corning 840 RESIN Medium-hard silicone binder resin for maintenance paints, colored baking enamels, decorative finishes. Improves heat resistance and weathering of organic resins. As an additive to improve flow-out o.. |
|||
Viscosity | 15 - 30 cP | 15 - 30 cP | |
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Sc.. |
|||
Viscosity | 5.0 - 30 cP | 5.0 - 30 cP | @ 275 |
ACC 1KSP EPI Engineered Polymers Silicone Polyurea Dispersion 1KSP is a silicone modified polyurea dispersion “Powered by ReactAmine® Technology” designed for a wide range of rigid and flexible substrates such as wood, metal, vinyl, concrete and other plast.. |
|||
Viscosity | 10 - 30 cP @Temperature 25.0 °C |
10 - 30 cP @Temperature 77.0 °F |
Uncured |
Permabond A126 Anaerobic Retainer Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u.. |