Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2650 cP | 2650 cP | |
Abatron AboCast 8110-9/AboCure 50-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |