Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 150000 - 260000 cP | 150000 - 260000 cP | |
Lord Adhesives 370 Two Component Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 200000 - 260000 cP | 200000 - 260000 cP | |
Lord Adhesives Metech 3501 Palladium Silver Conductor Composition Designed for use in the manufacture of hybrid circuitry, resistor networks, potentiometers as well as general purpose microcircuitry. It employs a conventional glass bonding mechanism, has wide proc.. |
|||
Viscosity | 200000 - 260000 cP | 200000 - 260000 cP | |
Lord Adhesives Metech 3502 Palladium Silver Conductor Composition Designed for use in the manufacture of hybrid circuitry, resistor networks, potentiometers as well as general purpose microcircuitry. It employs a conventional glass bonding mechanism, has wide proc.. |
|||
Viscosity | 200000 - 260000 cP | 200000 - 260000 cP | |
Lord Adhesives Metech 3503 Palladium Silver Conductor Composition Designed for use in the manufacture of hybrid circuitry, resistor networks, potentiometers as well as general purpose microcircuitry. It employs a conventional glass bonding mechanism, has wide proc.. |
|||
Viscosity | 200000 - 260000 cP | 200000 - 260000 cP | |
Lord Adhesives Metech 3504 Palladium Silver Conductor Composition Designed for use in the manufacture of hybrid circuitry, resistor networks, potentiometers as well as general purpose microcircuitry. It employs a conventional glass bonding mechanism, has wide proc.. |
|||
Viscosity | 200000 - 260000 cP | 200000 - 260000 cP | |
Lord Adhesives Metech 3505 Palladium Silver Conductor Composition Designed for use in the manufacture of hybrid circuitry, resistor networks, potentiometers as well as general purpose microcircuitry. It employs a conventional glass bonding mechanism, has wide proc.. |