Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 26 - 35 cP | 26 - 35 cP | |
Huntsman DY 9577 Epoxy Accelerator Mix Ratio with GY 6010 is 1.Comments/Applications: Casting, encapsulation, powder coatings, filament windings, pultrusion, molding, electrical tapes. Can be used as a catalyst. Latent at RT in GY.. |
|||
Viscosity | 26 cP @Temperature 21.0 °C |
26 cP @Temperature 69.8 °F |
|
H.C. Starck Baymetec® Tantalum Ethoxide |
|||
Viscosity | 26 cP | 26 cP | |
BASF Lupragen® N 700 1,8-Diazabicyclo-5,4,0-undecene-7 Formula: C7H18N2OCAS: 6674-22-2Description: Lupragen® N 700 –1,8-Diazabicyclo-5,4,0-undecene-7 is a colorless to yellowish liquid, with an amine-like odor. It is miscible with water in all propor.. |
|||
Viscosity | 26 cP | 26 cP | |
BASF Lupranate® 241 Isocyanate Description: Lupranate® 241 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high2,4’-MDI isomer content. Lupranate® 241 Isocyanate exhibits excellent low t.. |
|||
Viscosity | 26 cP | 26 cP | |
BASF Lupranate® 281 Isocyanate Description: Lupranate® 281 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric MDI) containing a very high amount of monomeric diphenylmethane diisocyanate (2,4'-MDI an.. |
|||
Viscosity | 26 cP | 26 cP | |
BASF Lupranate® 5220 Isocyanate Description: Lupranate® 5220 Isocyanate is a low viscosity polymeric MDI containing a high amount of diphenylmethane diisocyanate (monomeric MDI).Information provided by BASF |