Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 10 - 25 cP | 10 - 25 cP | |
Ritelok TL90 Post Assembly Threadlocker Anaerobic. Low viscosity threadlocker for port assembly. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant |
|||
Viscosity | 10 - 25 cP | 10 - 25 cP | |
ND Industries 150 Wicking Adhesive High Pressure Sealant Seals pores in welds and hairline cracks in castings |
|||
Viscosity | 10 - 25 cP | 10 - 25 cP | |
ND Industries 150 Wicking Adhesive Sealant Threadlocker General DescriptionMedium to high strength. Locks pre-assembled fasteners through capillary action and seals porosities in welds and hairline cracks in castings.Meets military spec MIL-S-46163 Type.. |
|||
Viscosity | 15 - 25 cP | 15 - 25 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 115 (20 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 5.0 - 25 cP | 5.0 - 25 cP | |
Huntsman Araldite DY 023 Reactive Diluent Weight per Epoxide (EEW, g/eq) 167 to 182. Max color is 1.Comments/Applications: Cresyl glycidyl ether - monofunctional epoxy. Less volatile and better resistance to water, but less efficient visc.. |
|||
Viscosity | 8.0 - 25 cP | 8.0 - 25 cP | As Supplied |
Heraeus Cleviosâ„¢ PH 500 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH 500 is an antistatic material based on PEDO.. |
|||
Viscosity | 10 - 25 cP @Temperature 25.0 °C |
10 - 25 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 24 LV General Purpose Catalyst Emerson & Cuming 24 LV Eccobond® General Purpose CatalystFaster curing, shorter working life version of 23 LV. Recommended for small mass castings due to higher exotherm. Cure Type: Room Temp or He.. |