Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 247500 cP @Temperature 25.0 °C |
247500 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 872-7TN1 Flexible Thixotropic Epoxy Adhesive TRA-BOND 872-7TN1 is a flexible thixotropic epoxy. The high viscosity and long worklife make this material easy to handle. Also, the high thermal conductivity makes this product ideal for electronic.. |