Polymer Property : Viscosity = 24500 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 24500 cP

@Temperature 25.0 °C
24500 cP

@Temperature 77.0 °F
Mixed (sp #7, 10 rpm)
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System
TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and ..