Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2250 cP | 2250 cP | Mixed |
Tra-Con Tra-Bond FS482 Long Pot Life High Tg Fiber Optic Epoxy Adhesive TRA-BOND FS-482 is a dark blue, low viscosity epoxy adhesive developed for fiber-optic bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, and other.. |
|||
Viscosity | 2250 - 12000 cP | 2250 - 12000 cP | Thixotropic |
Loctite® 243 Oil Resistant/Medium Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | >= 2250 cP | >= 2250 cP | |
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Viscosity | 2250 cP @Temperature 25.0 °C |
2250 cP @Temperature 77.0 °F |
at 100/13 (50-3/50-12) pbw |
Abatron AboCast 50-3/AboCure 50-12 Epoxy Data provided by the manufacturer, Abatron, Inc. Light motor oil viscosity, almost colorless. Shelf life is 12+ months. |