Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 140000 - 220000 cP | 140000 - 220000 cP | |
Lord Adhesives Metech 7806A Cermet Resistor Overglaze Composition Resistor overglaze composition 7806A is an acid resistant, laser trimable glaze designed to be printed and fired over thick film resistors. 7806A improves the stability of laser or air-abrasive trim.. |
|||
Viscosity | 180000 - 220000 cP | 180000 - 220000 cP | A |
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works.. |
|||
Viscosity | 180000 - 220000 cP | 180000 - 220000 cP | A |
ITW Plexus Plexusâ„¢ MA557 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Long working time, non-sagging, excellent g.. |
|||
Viscosity | 175000 - 220000 cP | 175000 - 220000 cP | A |
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois .. |
|||
Viscosity | 175000 - 220000 cP | 175000 - 220000 cP | B |
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois .. |
|||
Viscosity | 180000 - 220000 cP | 180000 - 220000 cP | A |
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works. |