Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.84 cP | 2.84 cP | 5% Toluene Solution; ASTM D445 |
LG Chemical LG-411 Styrene-Butadiene-Styrene Description: Radial structure, Non-Oil Extended Grade Thermoplastic ElastomerApplications: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS: 9003-55-8Information provided by LG Chem.. |