Polymer Property : Viscosity = 2.00e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin  (discontinued **)
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..
Viscosity 2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 4003 Anhydride-Modified HDPE Adhesive Resin  (discontinued **)
Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process..
Viscosity 2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi..
Viscosity 2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown
12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi..
Viscosity 2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
2.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Elvax® 3165 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3165 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Viscosity 2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Viscosity 2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
DSM Akulon® XP32-E1 PA6
Film Extrusion, Medium Viscosity, Lubricated, Nucleated
Viscosity 2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 280 °C
2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 536 °F
DSM Akulon® XP36-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Viscosity 2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
DSM Akulon® XP32-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Viscosity 2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 280 °C
2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 536 °F
DSM Akulon® XP36-E1 PA6
Film Extrusion, Medium Viscosity, Nucleated, Lubricated
Viscosity 2.00e+6 - 2.60e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
2.00e+6 - 2.60e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Viscosity 2.00e+6 - 2.50e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
2.00e+6 - 2.50e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 2751-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..
Viscosity 2.00e+6 - 2.50e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
2.00e+6 - 2.50e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..