Polymer Property : Viscosity = 1950 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 650 - 1950 cP
650 - 1950 cP
Lord Adhesives 312 General Purpose, Low Viscosity Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Viscosity 525 - 1950 cP
525 - 1950 cP
Thixotropic
Loctite® 641 Controlled Strength Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..