Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 10.0 - 180000 cP | 10.0 - 180000 cP | Average value: 20300 cP Grade Count:52 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |