Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 15 - 25 cP | 15 - 25 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 115 (20 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | <= 15 cP | <= 15 cP | |
Huntsman Araldite DY 025 Reactive Diluent Weight per Epoxide (EEW, g/eq) 280 to 315. Max color is 1.Comments/Applications: Epoxide 8: Aliphatic glycidyl ether consisting primarily of C12 and C14 alkyl groups. Monofunctional. Efficient vi.. |
|||
Viscosity | <= 15 cP | <= 15 cP | |
Huntsman Araldite DY 027 Reactive Diluent Weight per Epoxide (EEW, g/eq) 220 to 250. Max color is 1.Comments/Applications: Epoxide 7: Monofunctional. Alkyl glycidyl ether - alkyl groups are predominantly C8 and C10. Very effective viscos.. |
|||
Viscosity | 15 - 35 cP | 15 - 35 cP | |
Lord Adhesives 551 Very Low Viscosity, Adhesive Thinner, Medium Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Viscosity | 15 - 50 cP | 15 - 50 cP | As Supplied |
Heraeus Cleviosâ„¢ PH 1000 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH 1000 is an antistatic material based on PED.. |
|||
Viscosity | 15 - 30 cP | 15 - 30 cP | |
Shandong Dongyue Polymer DF-302 PTFE Aqueous Dispersion 60% Usage: The resin is used for impregnating porous material, such as asbestos, fiberglass, anti-corrosive, abrasion resistant, filature and lubricating materials.Packing: The PTFE is packed in PVC cir.. |
|||
Viscosity | 15 - 20 cP @Temperature 120 °C |
15 - 20 cP @Temperature 248 °F |
|
Struktol MONTAN WAX E Lubricant, Processing Additive Montanic ester wax.STRUKTOL® Montan Wax E is an excellent processing additive for PVC. It provides superior plate out properties, wide processing latitude and is ideal for clear applications. Pri.. |
|||
Viscosity | 15 - 30 cP | 15 - 30 cP | |
Shandong Dongyue Polymer DF-301 PTFE Aqueous Dispersion 60% Usage: The resin is used for impregnating porous material, such as asbestos, fiberglass, anti-corrosive, abrasion resistant, filature and lubricating materials.Packing: The PTFE is packed in PVC cir.. |
|||
Viscosity | 15 cP @Temperature 200 °C |
15 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3300 Polyester, Flake Low molecular weight type UE3210, High OH type, Branched & highly crosslinkedUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications fro.. |
|||
Viscosity | 15 cP @Temperature 200 °C |
15 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3380 Polyester, Flake Low molecular weight type UE3200, Low softening point, High OH typeUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products.. |
|||
Viscosity | 15 cP | 15 cP | |
Zircar Refractory Composites SI-HARD SILICA RIGIDIZER HARDENER ZRCI SI-HARD Rigidizer Hardener is a alkaline, aqueous dispersion of colloidal silica at 50% concentration. The dispersed silica is present as amorphous spheres, 100 nanometers in size. The silica p.. |
|||
Viscosity | 15 cP | 15 cP | |
BASF Lupranate® 227 Isocyanate Description: Lupranate® 227 Isocyanate is a liquid, modified blend product based on isomers of diphenylmethane diisocyanate (MDI). This product has good storage stability at room temperature and of.. |
|||
Viscosity | 15 - 40 cP | 15 - 40 cP | |
3M Pronto™ CA-7 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting product with .. |
|||
Viscosity | 15 - 30 cP | 15 - 30 cP | |
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Sc.. |
|||
Viscosity | 15 - 40 cP | 15 - 40 cP | |
3M Scotch-Weld™ CA7 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to metals, plastics, and rubbers.Information provided by 3.. |
|||
Viscosity | 15 cP | 15 cP | QSil 12C |
ACC QSil 12 QSI Quantum Silicones Clear Low Viscosity for Potting Material QSil 12 is a clear, transparent, low viscosity, two-component, liquid silicone material which cures at room temperature and is primarily intended for potting applications. This material is typically.. |
|||
Viscosity | 15 cP | 15 cP | Extrusion rate, 25C, 30 psi, 15 gauge needle |
Loctite® 5071 Silicone Encapsulant Conformal CoatingsConformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Locti.. |